What are Copper Nanoparticles ?
Copper (Cu) Nanoparticles are black brown spherical high surface area metal particles. Nanoscale Copper Particles are typically 10-30 nanometers (nm) with specific surface area (SSA) in the 30 - 70 m2/g range and also available in with an average particle size of 70 -100 nm range with a specific surface area of approximately 5 - 10 m2/g.
Nano Copper Particles are also available in passivated and in Ultra high purity and high purity and carbon coated and dispersed forms. They are also available as a nanofluid through the AE Nanofluid production group. Nanofluids are generally defined as suspended nanoparticles in solution either using surfactant or surface charge technology. Nanofluid dispersion and coating selection technical guidance is also available.
You might also like
| Magnetic Nanoparticle What is Magnetic Nanoparticle ? When a piece... | What is Nanoparticle ? Nanoparticles - a Definition Nanoparticles... | Silver Nanoparticle What is Silver Nanoparticles ? Silver nanoparticles... | Nanomaterials - the Future Technology Nanomaterials - Applications for Nanotechnology Nanomaterials... |





Alloy Suppliers
Aluminum
Aluminum Extrusions
Copper-Brass-Bronze
Nickel
Magnets
Stainless Steel
Stainless Steel Tubing
Steel Service Centers
Titanium
Tungsten
Wire Rope