Introduction:
A bearing that had been in service for a year and a half was sent to undergo failure analysis (Figure 1). This bearing had been installed in the drive centrifugal pump in the R-8 plant.
Figure 1. Photograph of bearing setup
Figure 2. Photograph of inner ring showing spalling in groove
Figure 3. SEM photograph of spalling, flaking and cracking, in the groove. 200X